Product parameter


Inner tank material : SUS304 stainless steel ,0.5-0.6mm in thickness.

Insulation material : polyurethane foaming,60mm in thickness

Outer tank material :plastic coated galvanized steel plate ,0.5mm in thickness.Frame material : plastic coated galvanized steel plate ,2.0mm in thickness.

Vacuum tube material :borosilicate glass 3.3, the vacuum degree of evacuated tube is less than 5×10-4pa, emission ratio ≤0.04

Power of electrical heating element : 1) No. of vacuum tube ≤18, P=1.5kw  2) No. of vacuum tube

≥20, P=2.4kw


Core advantages of our products


1.     Evacuated tube coating technology – interference film coating

UTLE solar vacuum tube obsoletes the traditional gradual film coating and applies the world'smost advanced vacuum tube coating technology – interference film coating, the three target coating - aluminum, copper and stainless steel. The gradual selective absorbing film coating with a gently curve, the emittance increase a lot when the working temperature rise to 300 - 500 ℃ as the emittance increase when the temperature rises. However, Himin "three-high" solar vacuum tube with interference absorption ultra-low emission selective absorption layer can solve the above problem instead of the gradual film coating.

2.    Argon tungsten-arc welding technology of inner tank

1)Argon tungsten-arc welding technology is adopted for the welding of inner tank.

2)Before welding,wipe the inner tank plate with appropriative clean fluid, and do the welding within 10 minutes.

3)The material of inner tank is sus 304 with high content of nickel (9%)and chromium(18%),


and the thickness of the plate is 0.5mm

3.   Advanced surface treatment process of bracket and shell-electrostatic spraying and high temperature solidification.


There are 16 surface treatment process.Technological process:put up the workpiece,degrease in advance, degrease, water cleaning1, water cleaning 2, pure water cleaning, vitrification, water cleaning1, water cleaning 2, pure water cleaning2, pure water spraying, drying,  solidification(200℃,15 minutes)take down the workpiece, trail assembly,final assembly.

4.   Polyurethane horizontal type foaming coating patent technology

1)Controlled by micro-computer, thermostatic quantitative high pressure one-time foaming process is used, and next high temperature solidification treatment is done.

2) Himin unique horizontal foaming technology, making the foaming more uniform.

3)Imported polyurethane foaming material.


4)The foaming density is a gold density , it reaches 40kg/m3.